Vancouver, B.C. (April 15, 2021) – First Energy Metals Ltd. (CSE: FE) ("First Energy" or the “Company) is pleased to announce assay results of another round of grab and channel sampling from the Augustus Lithium Property in Quebec, Canada. A total of 24 grab and channel samples of varying lengths were cut out of Beluga Pegmatite Zone with a surface exposure of over 100 metres wide and 250 m along strike located at the Canadian Lithium Prospect. The present sampling represents 10.64 metres of channel sampling in the southern part of the Beluga Pegmatite. The field crew is continuously cutting and sampling the remaining outcrops which will be reported as soon as the results are available. Three out of four grab samples assayed up to 4.61 percent (%) lithium oxide (Li2O) with an average value of 3.04% Li2O while the fourth sample returned a low value of 12 ppm lithium. Results of channel sampling completed so far on Beluga Pegmatite indicate a width of 10.64 metres at 0.24% Li2O.
Highlights of Channel Samples Assays (see Table 1 for details)
- Lithium (Li) values are in the range of 34 ppm (parts per million) to 4,020 ppm (0.4% Li) with an average of 1,051.70 ppm, where seven samples are over 1,000 ppm lithium.
- Lithium oxide (Li2O) values are in the range of 0.001% to 0.87% Li2O with a total width of 10.64 metres at 0.24% Li2O.
- Beryllium values are in the range of 103 ppm to 574 ppm, cesium is in the range of 6.6 ppm to 83.9 ppm, and niobium is from 51 ppm to 87.1 ppm.
- Rubidium is in the range of 58.4 ppm to 2,720 ppm, tantalum is 44.7 ppm 81.3 ppm, and barium from 24 ppm to 113 ppm.
The ground exploration work has been continuous since February 2021 and its purpose is to locate and confirm historical lithium pegmatite occurrences on two lithium prospects (Augustus and Canadian Lithium Prospects), to locate historical drill holes on the Property completed in 1950’s, and to support the ongoing drill program. The pegmatite outcrops are exposed using an excavator, and several historical drill hole casings were located which are useful guidelines for placing drill holes and mapping lithium pegmatites on surface. The field exploration is continuous, and more channel sampling is being carried out on the exposed outcrops.
Each channel sample from this program represents about 0.26 – 0.87 cm long, 5 cm wide and 3-5 cm deep cut in bedrock. Grab samples are selected samples and are not necessarily representative of the mineralization hosted on the property. The samples were bagged and tagged using best practices and were delivered to Activation Laboratories (“ACTLABS”), Ancaster, Ontario for sample preparation and analyses using laboratories code Ultratrace 7 as summarized below. ACTLABS is an independent commercial, accredited ISO Certified Laboratory.
Code Ultratrace 7 – Peroxide Fusion – ICP and ICP/MS
Samples are fused with sodium peroxide in a Zirconium crucible. The fused sample is acidified with concentrated nitric and hydrochloric acids. The resulting solutions are diluted and then measured by ICP-OES and ICP-MS. All metals are solubilized.
ICP-MS
Fused samples are diluted and analyzed by Agilent 7900 ICP-MS. Calibration is performed using five synthetic calibration standards. A set of (10-20) fused certified reference material is run with every batch of samples for calibration and quality control. Fused duplicates are run every 10 samples.
ICP-OES
Samples are analyzed with a minimum of 10 certified reference materials for the required analytes, all prepared by sodium peroxide fusion. Every 10th sample is prepared and analyzed in duplicate; a blank is prepared every 30 samples and analyzed. Samples are analyzed using a Varian 735ES ICP and internal standards are used as part of the standard operating procedure. Source: https://actlabs.com/geochemistry/lithogeochemistry-and-whole-rock-analysis/peroxide-total-fusion/
Afzaal Pirzada, P.Geo., Geological Consultant of the Company, and a “Qualified Person” for the purposes of National Instrument 43-101 - Standards of Disclosure for Mineral Projects, has reviewed and approved the scientific and technical information contained in this news release.
About the Augustus Lithium Property
The Company owns 100% interest in Augustus Lithium Property in Landrienne & Lacorne-Townships, Quebec, Canada. The Property consists of 271 mining claims covering a total area of 14,155 hectares located approximately 40 kilometres northwest of the town of Val d’Or on map sheets 32C/05 and 32D08. The Property claims are spread in several claim blocks optioned in 2021 from different vendors. The Company has prepared a well thought out work plan on the property which includes diamond drilling, metallurgical testwork to produce battery grade lithium carbonate, and resource estimation. To date, the Company has compiled historical drill hole data on the Property for 74 historical dill holes with a cumulative drilling of 12,123.14 m, out which 6,024 m drilling was completed on the two lithium prospects on the Property. Several drill hole results indicated intersections over 1% lithium oxide. All this data is helpful in developing and executing the current exploratory drill program and building a data base for NI 43-101 resource estimation”.
About First Energy Metals Limited.
First Energy Metals is a Canadian mineral exploration company with a primary focus of acquiring a multicommodity mineral property portfolio. Its goal is to identify, acquire and explore North American mineral prospects in the technology metals, precious metal, and base metal sector.
The company's strategy is to:
- Acquire and advance projects through prospecting and early-stage exploration;
- Source joint venture partners to finance future exploration and project development;
- Create shareholder value through exploration success.
First Energy will continue to add to its multicommodity portfolio through organic acquisitions of new projects and opportunities with the intention of adding value and projects over time.
ON BEHALF OF THE BOARD OF
FIRST ENERGY METALS LTD.
"Gurminder Sangha"
Gurminder Sangha
President & Chief Executive Officer
For further information, please contact the Company at: gsangha@firstenergymetals.com
Neither the Canadian Securities Exchange (CSE) nor its Regulation Services Provider accepts responsibility for the adequacy or accuracy of this news release and has neither approved nor disapproved the contents of this news release.
Forward-looking Information
Except for the statements of historical fact, this news release contains “forward-looking information” within the meaning of the applicable Canadian securities legislation that is based on expectations, estimates and projections as at the date of this news release. “Forward-looking information” in this news release includes information about the Company’s information concerning the intentions, plans and future actions of the parties to the transactions described herein and the terms thereon.
The forward-looking information in this news release reflects the current expectations, assumptions and/or beliefs of the Company based on information currently available to the Company. In connection with the forward-looking information contained in this news release, the Company has made assumptions about the Company’s ability to obtain required approvals. The Company has also assumed that no significant events occur outside of the Company's normal course of business. Although the Company believes that the assumptions inherent in the forward-looking information are reasonable, forward-looking information is not a guarantee of future performance and accordingly undue reliance should not be put on such information due to the inherent uncertainty therein.
Table 1: Sample assays highlights
Analyte Symbol
Location NAD 1983 UTM Zone 18
Sample type / Length in m
Ba
Be
Cs
Li
Li2O
Nb
Rb
Ta
Unit Symbol
ppm
ppm
ppm
ppm
%
ppm
ppm
ppm
Detection Limit
3
3
0.1
3
2.4
0.4
0.2
Analysis Method
Easting
Northing
FUS-MS-Na2O2
1387930
286876
5367948
0.84
24
206
6.6
34
0.01
72.2
74.7
62.3
1387931
286878
5367947
0.44
36
282
14.1
38
0.01
86.2
377
60.5
1387932
286879
5367948
0.6
57
316
35.2
1640
0.35
71
879
44.9
1387933
286881
5367947
0.87
42
574
46.8
1030
0.22
69
1030
53.6
1387934
286879
5367947
0.8
61
211
60.1
3250
0.70
65.9
2140
50.4
1387935
286884
5367947
0.73
113
228
83.9
403
0.09
67.8
2720
68.8
1387936
286883
5367950
0.88
47
280
46
285
0.06
78.9
1650
72.7
1387937
286884
5367948
0.47
38
218
50
3530
0.76
75.1
1630
81.3
1387938
286885
5367948
0.51
21
421
37.3
738
0.16
59.1
600
64.7
1387939
286885
5367948
0.46
36
485
28.7
74
0.02
51.9
323
53.9
1387940
286886
5367949
0.46
12
162
9.9
36
0.01
47.8
59.2
52.7
1387941
286886
5367949
0.4
43
103
12
19
0.00
61.1
216
60.1
1387943
286878
5367954
0.51
27
349
53
197
0.04
67.9
1790
71.4
1387944
286878
5367954
0.5
17
249
36.7
1600
0.34
76.3
1110
65.7
1387945
286881
5367952
0.53
33
618
63.2
2420
0.52
51
1430
44.7
1387946
286880
5367958
0.52
54
325
63.1
563
0.12
61.1
1750
62.2
1387947
286895
5367927
0.6
36
234
51.3
4020
0.87
87.1
1460
53.7
1387948
286895
5367925
0.26
17
288
8.8
46
0.01
76.9
58.4
71.5
1387949
286891
5367938
0.26
62
321
45.6
59
0.01
69.7
1240
51.4
Total 10.64 metres @ 0.24% lithium oxide
Grab Samples
1387942
286893
5367934
Grab
56
204
31.6
12
0.00
69.4
1470
47
95664
284902
5368374
Grab
15
168
46.8
15200
3.27
90.1
1040
91.4
95665
284882
5368370
Grab
14
468
112
5800
1.25
58.6
2840
61.8
95666
284930
5368312
Grab
9
63
50.3
21400
4.61
28.2
1290
18.3
Note: A standard conversion factor of 2.153 was used to report Li to Li2O values